可逆凝胶
- 网络reversible gel

-
形成热不可逆凝胶的工艺条件是:预煮时间为28min,氢氧化钙浓度为0.06%,预煮温度为90℃。
The process condition to form thermo-irreversible gels is : the precook time is 28 minutes , the concentration of calcium hydroxide is 0.06 % and the precook temperature is 90 ℃ .
-
结果表明:体系的温度升高和降低时,凝胶可发生热可逆溶胶-凝胶相互转变;
The results showed that the systems underwent the sol-gel transition with the increase and decrease of the temperature .