摩擦色牢度
- 网络RUBBING;rubbing fastness;rubbing/crocking
-
结果表明,环保型助剂ZNL可明显降低分散染料热溶染色温度,提高织物的匀染性和透染性,改善织物的耐摩擦色牢度,且对织物强力和皂洗牢度影响较小。
As a result , the ecological auxiliary ZNL can greatly reduce the temperature of thermosol dyeing , increase the levelness and penetration , and improve rubbing fastness , and less effect on fabric strength and color fastness to soaping .
-
湿摩擦色牢度和水洗牢度增加。深浓色纯棉织物的湿摩擦牢度
The rubbing fastness and washing resistance are elevated . Color fastness to wet crocking of cotton fabric in deep shade
-
粘合剂的Tg在-10℃左右可得到好的手感和干、湿摩擦色牢度。
Binding agent with the Tg of about - 10'C could make the printed fabrics have a good handle and suit - able dry and wet crocking colour fastness .
-
纺织品耐有机溶剂摩擦色牢度:全氯乙烯法
Testing method for colorfastness to solvent spotting : perchloroethylene method
-
纺织品耐摩擦色牢度测试方法的差异比较
Comparison between Different Testing Methods for Color Fastness to Rubbing
-
皮革耐摩擦色牢度的测定
Testing method for colour fastness to rubbing of leathers
-
主要用于染色纤维制品的耐摩擦色牢度的评价和判定。
Mainly used in dyeing fibre products of friction resistance fastness of evaluation and judgement .
-
GB/T17530.3-1998工业丙烯酸及酯色度的测定皮革耐摩擦色牢度的测定
Acrylic acid and acrylate esters for industrial use-Determination of color testing method for colour fastness to rubbing of leathers
-
染后耐洗及耐摩擦色牢度均达到4级以上,耐光色牢度为3级。
The color fastness to washing and rubbing reached up to 4-level , but the fastness to light was only 3-level .
-
先染色再抗静电整理的涤纶具有增深效果、良好的摩擦色牢度和抗静电性能。
The polyester fibers dyed before antistatic finishing had not only dark effect but also good abrasion fastness and antistatic properties .
-
染色、抗静电同浴整理相对涤纶织物直接染色的颜色浅,且抗静电性能和摩擦色牢度良好。
One-bath dyed-antistatic finished polyester fibers had lighter colors than directly dyed fibers , but the antistatic effect and abrasion fastness were good .
-
经高粱红铁媒染后的羊毛织物干、湿摩擦色牢度和皂洗色牢度均较好,达到4级,说明该染料适用于羊毛织物的染色。
The rubbing and washing color fastness of dyed wool fabric were all 4 or up to 4.It indicated that sorghum red dye was suitable to dye wool fabric .
-
试验结果表明:直接染色样品的摩擦色牢度3~4级,皂洗色牢度3~4级,铁媒染后摩擦色牢度和皂洗色牢度提高为4级。
The results showed that the directly dyed samples had rate 3 ~ 4 rubbing and soaping color fastnesses , and the iron mordant dyed ones had rate 4 rubbing and soaping fastnesses .