At reduced environment the content of As increases from 51.82 % at temperature of 1300K to 97.28 % at 1600K , while the content of As is only 0.19 % in melted oxides .
在还原气氛下,在1300~1600K温度范围内,As在气相的含量由1300K时的51.82%升高至1600K时的97.28%,而在氧化物熔融体中的含量只有0.19%。
-
We study the process of rapid quenching of the liquid iron at 2200K through 2000K , 1800K , 1600K to 1400K and then obtain the statistical analysis of the pair distribution function , mean square displacement , correlation and the Voronoi polyhedra at the temperature equilibrium state .
研究了液态铁在2200K下淬火,经过2000K、1800K、1600K至1400K的过程,并统计分析了各温度平衡态的双体分布函数、均方位移、配位数、及对Voronoi多面体进行分析。